abs-novodur
novodur regrind
thin lack
Related products
Carbon Black
High Grade Carbon black. No CC. Carbon 70% USAGE less than 1% Shinny and Black Suitable use for pelletized: ABS / PS / PP / HDPE etc
PVC Regrind
Regrind Recycled Plastic Post PVC Scrap
PP Skid Regrinds
Ongoing PP Skid Regrinds
Melt range 4-10
PVC From Pipes
Long Service Life Pvc Particles Nice Price Pvc Particles High Elastic And Environmentally Pvc Particles
Pet Flakes
Bottles made of polyethylene terephthalate can be used to make lower grade products, such as carpets. To make a food grade plastic, the bottles need to be hydrolysed down to monomers, which are purified and then re-polymerised to make new PET.
PE100 pipe shred
Storing bags 25kg available
We have jumbo bags and 25kg bags with ldpe linner or without ldpe linner kindly contact for more details
Recycled Pp Granules Black Color
Recycled Polypropylene PP Granules
Post-industrial recycled PP granules.
Recycled PP granules from thermoformed food contact containers.
High quality, produced only from industrial sources.
Colour: Black
Melt Flow Index: 3-4 g/10min
Loading weight: 24-25 Tonnes
Packaging,: Big-bags
Vampamid 6 0024 V0 PA6 Grey
Specifications on the attached image.
12 pallets in stock
EPE Hot Melt Blocks
30,000lbs EPE Hot Melt Blocks
Recently Viewed
abs-novodur
novodur regrind
thin lack
PE 80+100 Repro
Free Sample High Density Polyethylene Resin HDPE PE100 Virgin HDPE Granules recycled virgin HDPE resin
|
Film Grade HDPE
|
||||
|
Item
|
Test Condition
|
Test Method
|
Value
|
Unit
|
|
Density
|
ISO 1183
|
0.944-0.955
|
g/cm3
|
|
|
MFR
|
190°C/2.16kg
|
ISO 1133
|
0.03-0.07
|
g/10min
|
|
Tensile Strength at Yield
|
ISO 527-2
|
22
|
MPa
|
|
|
Elongation at break
|
ISO 527-2
|
>350
|
%
|
|
|
ESCR
|
F50,50°C,100%
|
ASTM D-1693A
|
1000
|
h
|
|
VICAT
|
ASTM D-1525
|
126
|
°C
|
|
|
Blowing molding Grade HDPE
|
||||
|
Item
|
Test Condition
|
Test Method
|
Value
|
Unit
|
|
Density
|
ISO 1183
|
0.950~0.955
|
g/cm
|
|
|
MFR
|
190°C/2.16kg
|
ISO 1133
|
1.7~2.5
|
g/10min
|
|
Tensile strength at Yield
|
ISO 527-2
|
24
|
MPa
|
|
|
Elongation at break
|
ISO 527-2
|
>600
|
%
|
|